• Understanding the transfer of spin angular momentum is essential in modern magnetism research. A model case is the generation of magnons in magnetic insulators by heating an adjacent metal film. Here, we reveal the initial steps of this spin Seebeck effect with <27fs time resolution using terahertz spectroscopy on bilayers of ferrimagnetic yttrium-iron garnet and platinum. Upon exciting the metal with an infrared laser pulse, a spin Seebeck current $j_\textrm{s}$ arises on the same ~100fs time scale on which the metal electrons thermalize. This observation highlights that efficient spin transfer critically relies on carrier multiplication and is driven by conduction electrons scattering off the metal-insulator interface. Analytical modeling shows that the electrons' dynamics are almost instantaneously imprinted onto $j_\textrm{s}$ because their spins have a correlation time of only ~4fs and deflect the ferrimagnetic moments without inertia. Applications in material characterization, interface probing, spin-noise spectroscopy and terahertz spin pumping emerge.
  • Recent studies have shown that material structures, which lack structural inversion symmetry and have high spin-orbit coupling can exhibit chiral magnetic textures and skyrmions which could be a key component for next generation storage devices. The Dzyaloshinskii-Moriya Interaction (DMI) that stabilizes skyrmions is an anti-symmetric exchange interaction favoring non-collinear orientation of neighboring spins. It has been shown that material systems with high DMI can lead to very efficient domain wall and skyrmion motion by spin-orbit torques. To engineer such devices, it is important to quantify the DMI for a given material system. Here we extract the DMI at the Heavy Metal (HM) /Ferromagnet (FM) interface using two complementary measurement schemes namely asymmetric domain wall motion and the magnetic stripe annihilation. By using the two different measurement schemes, we find for W(5 nm)/Co20Fe60B20(0.6 nm)/MgO(2 nm) the DMI to be 0.68 +/- 0.05 mJ/m2 and 0.73 +/- 0.5 mJ/m2, respectively. Furthermore, we show that this DMI stabilizes skyrmions at room temperature and that there is a strong dependence of the DMI on the relative composition of the CoFeB alloy. Finally we optimize the layers and the interfaces using different growth conditions and demonstrate that a higher deposition rate leads to a more uniform film with reduced pinning and skyrmions that can be manipulated by Spin-Orbit Torques.
  • GRAVITY Collaboration: R. Abuter, M. Accardo, A. Amorim, N. Anugu, G. Ávila, N. Azouaoui, M. Benisty, J.P. Berger, N. Blind, H. Bonnet, P. Bourget, W. Brandner, R. Brast, A. Buron, L. Burtscher, F. Cassaing, F. Chapron, É. Choquet, Y. Clénet, C. Collin, V. Coudé du Foresto, W. de Wit, P.T. de Zeeuw, C. Deen, F. Delplancke-Ströbele, R. Dembet, F. Derie, J. Dexter, G. Duvert, M. Ebert, A. Eckart, F. Eisenhauer, M. Esselborn, P. Fédou, G. Finger, P. Garcia, C.E. Garcia Dabo, R. Garcia Lopez, E. Gendron, R. Genzel, S. Gillessen, F. Gonte, P. Gordo, M. Grould, U. Grözinger, S. Guieu, P. Haguenauer, O. Hans, X. Haubois, M. Haug, F. Haussmann, Th. Henning, S. Hippler, M. Horrobin, A. Huber, Z. Hubert, N. Hubin, C.A. Hummel, G. Jakob, A. Janssen, L. Jochum, L. Jocou, A. Kaufer, S. Kellner, L. Kern, P. Kervella, M. Kiekebusch, R. Klein, Y. Kok, J. Kolb, M. Kulas, S. Lacour, V. Lapeyrère, B. Lazareff, J.-B. Le Bouquin, P. Lèna, R. Lenzen, S. Lévêque, M. Lippa, Y. Magnard, L. Mehrgan, M. Mellein, A. Mérand, J. Moreno-Ventas, T. Moulin, E. Müller, F. Müller, U. Neumann, S. Oberti, T. Ott, L. Pallanca, J. Panduro, L. Pasquini, T. Paumard, I. Percheron, K. Perraut, G. Perrin, A. Pflüger, O. Pfuhl, T. Phan Duc, P.M. Plewa, D. Popovic, S. Rabien, A. Ramírez, J. Ramos, C. Rau, M. Riquelme, R.-R. Rohloff, G. Rousset, J. Sanchez-Bermudez, S. Scheithauer, M. Schöller, N. Schuhler, J. Spyromilio, C. Straubmeier, E. Sturm, M. Suarez, K.R.W. Tristram, N. Ventura, F. Vincent, I. Waisberg, I. Wank, J. Weber, E. Wieprecht, M. Wiest, E. Wiezorrek, M. Wittkowski, J. Woillez, B. Wolff, S. Yazici, D. Ziegler, G. Zins
    May 5, 2017 astro-ph.IM
    GRAVITY is a new instrument to coherently combine the light of the European Southern Observatory Very Large Telescope Interferometer to form a telescope with an equivalent 130 m diameter angular resolution and a collecting area of 200 m$^2$. The instrument comprises fiber fed integrated optics beam combination, high resolution spectroscopy, built-in beam analysis and control, near-infrared wavefront sensing, phase-tracking, dual beam operation and laser metrology [...]. This article gives an overview of GRAVITY and reports on the performance and the first astronomical observations during commissioning in 2015/16. We demonstrate phase tracking on stars as faint as m$_K$ ~ 10 mag, phase-referenced interferometry of objects fainter than m$_K$ ~ 15 mag with a limiting magnitude of m$_K$ ~ 17 mag, minute long coherent integrations, a visibility accuracy of better than 0.25 %, and spectro-differential phase and closure phase accuracy better than 0.5{\deg}, corresponding to a differential astrometric precision of better than 10 microarcseconds ({\mu}as). The dual-beam astrometry, measuring the phase difference of two objects with laser metrology, is still under commissioning. First observations show residuals as low as 50 {\mu}as when following objects over several months. We illustrate the instrument performance with the observations of archetypical objects for the different instrument modes. Examples include the Galactic Center supermassive black hole and its fast orbiting star S2 for phase referenced dual beam observations and infrared wavefront sensing, the High Mass X-Ray Binary BP Cru and the Active Galactic Nucleus of PDS 456 for few {\mu}as spectro-differential astrometry, the T Tauri star S CrA for a spectro-differential visibility analysis, {\xi} Tel and 24 Cap for high accuracy visibility observations, and {\eta} Car for interferometric imaging with GRAVITY.
  • To explore the capabilities of metallic spintronic thin-film stacks as a source of intense and broadband terahertz electromagnetic fields, we excite a W/CoFeB/Pt trilayer on a large-area glass substrate (diameter of 7.5 cm) by a femtosecond laser pulse (energy 5.5 mJ, duration 40 fs, wavelength 800 nm). After focusing, the emitted terahertz pulse is measured to have a duration of 230 fs, a peak field of 300 kV cm$^{-1}$ and an energy of 5 nJ. In particular, the waveform exhibits a gapless spectrum extending from 1 to 10 THz at 10% of amplitude maximum, thereby facilitating nonlinear control over matter in this difficult-to-reach frequency range and on the sub-picosecond time scale.
  • A thorough understanding of the mean-free-path (MFP) distribution of the energy carriers is crucial to engineer and tune the transport properties of materials. In this context, a significant body of work has investigated the phonon and electron MFP distribution, however, similar studies of the magnon MFP distribution have not been carried out so far. In this work, we used thickness-dependence measurements of the longitudinal spin Seebeck (LSSE) effect of yttrium iron garnet films to reconstruct the cumulative distribution of a SSE related effective magnon MFP. By using the experimental data reported by Guo et al. [Phys. Rev. X 6, 031012 (2016)], we adapted the phonon MFP reconstruction algorithm proposed by A.J. Minnich, [Phys. Rev. Lett. 109, 205901 (2012)] and apply it to magnons. The reconstruction showed that magnons with different MFP contribute in different manner to the total LSSE and the effective magnon MFP distribution spreads far beyond their typical averaged values.
  • Terahertz electromagnetic radiation is extremely useful for numerous applications such as imaging and spectroscopy. Therefore, it is highly desirable to have an efficient table-top emitter covering the 1-to-30-THz window whilst being driven by a low-cost, low-power femtosecond laser oscillator. So far, all solid-state emitters solely exploit physics related to the electron charge and deliver emission spectra with substantial gaps. Here, we take advantage of the electron spin to realize a conceptually new terahertz source which relies on tailored fundamental spintronic and photonic phenomena in magnetic metal multilayers: ultrafast photo-induced spin currents, the inverse spin-Hall effect and a broadband Fabry-P\'erot resonance. Guided by an analytical model, such spintronic route offers unique possibilities for systematic optimization. We find that a 5.8-nm-thick W/CoFeB/Pt trilayer generates ultrashort pulses fully covering the 1-to-30-THz range. Our novel source outperforms laser-oscillator-driven emitters such as ZnTe(110) crystals in terms of bandwidth, terahertz-field amplitude, flexibility, scalability and cost.
  • MATISSE is the second-generation mid-infrared spectrograph and imager for the Very Large Telescope Interferometer (VLTI) at Paranal. This new interferometric instrument will allow significant advances by opening new avenues in various fundamental research fields: studying the planet-forming region of disks around young stellar objects, understanding the surface structures and mass loss phenomena affecting evolved stars, and probing the environments of black holes in active galactic nuclei. As a first breakthrough, MATISSE will enlarge the spectral domain of current optical interferometers by offering the L and M bands in addition to the N band. This will open a wide wavelength domain, ranging from 2.8 to 13 um, exploring angular scales as small as 3 mas (L band) / 10 mas (N band). As a second breakthrough, MATISSE will allow mid-infrared imaging - closure-phase aperture-synthesis imaging - with up to four Unit Telescopes (UT) or Auxiliary Telescopes (AT) of the VLTI. Moreover, MATISSE will offer a spectral resolution range from R ~ 30 to R ~ 5000. Here, we present one of the main science objectives, the study of protoplanetary disks, that has driven the instrument design and motivated several VLTI upgrades (GRA4MAT and NAOMI). We introduce the physical concept of MATISSE including a description of the signal on the detectors and an evaluation of the expected performances. We also discuss the current status of the MATISSE instrument, which is entering its testing phase, and the foreseen schedule for the next two years that will lead to the first light at Paranal.
  • Thin film YIG (Y$_3$Fe$_5$O$_{12}$) is a prototypical material for experiments on thermally generated pure spin currents and the spin Seebeck effect. The 3-omega method is an established technique to measure the cross-plane thermal conductance of thin films, but can not be used in YIG/GGG (Ga$_3$Gd$_5$O$_{12}$) systems in its standard form. We use two-dimensional modeling of heat transport and introduce a technique based on Bayesian statistics to evaluate measurement data taken from the 3-omega method. Our analysis method allows us to study materials systems that have not been accessible with the conventionally used 3-omega analysis. Temperature dependent thermal conductance data of thin film YIG are of major importance for experiments in the field of spin-caloritronics. Here we show data between room temperature and 10 K for films covering a wide thickness range as well as the magnetic field effect on the thermal conductance between 10 K and 50 K.
  • Magnetic shape memory Heusler alloys are multiferroics stabilized by the correlations between electronic, magnetic and structural order. To study these correlations we use time resolved x-ray diffraction and magneto-optical Kerr effect experiments to measure the laser induced dynamics in a Heusler alloy Ni$_2$MnGa film and reveal a set of timescales intrinsic to the system. We observe a coherent phonon which we identify as the amplitudon of the modulated structure and an ultrafast phase transition leading to a quenching of the incommensurate modulation within 300~fs with a recovery time of a few ps. The thermally driven martensitic transition to the high temperature cubic phase proceeds via nucleation within a few ps and domain growth limited by the speed of sound. The demagnetization time is 320~fs, which is comparable to the quenching of the structural modulation.
  • We report on magnetization data obtained as a function of temperature and magnetic field in Li2 (Pd0.8Pt0.2)3B and Li2Pd3B non-centro-symmetric superconductors. Reversible magnetization curves were plotted as M1/2 vs. T. This allows study of the asymptotic behavior of the averaged order parameter amplitude (gap) near the superconducting transition. Results of the analysis show, as expected, a mean field superconducting transition for Li2Pd3B. On contrary, a large deviation from the mean field behavior is revealed for Li2(Pd0.8Pt0.2)3B. This is interpreted as due to the strength of the non s-wave spin-triplet pairing in this Pt-containing compound which produces nodes in the order parameter and consequently, phase fluctuations. The diamagnetic signal above Tc(H) in Li2Pd3B is well explained by superconducting Gaussian fluctuations, which agrees with the observed mean field transition. For Li2(Pd0.8Pt0.2)3B the diamagnetic signal above Tc(H) is much higher than the expected Gaussian values and appears to be well explained by three dimensional critical fluctuations of the lowest-Landau-level type, which somehow agrees with the scenario of a phase mediated transition.
  • The Photodetector Array Camera and Spectrometer (PACS) is one of the three science instruments on ESA's far infrared and submillimetre observatory. It employs two Ge:Ga photoconductor arrays (stressed and unstressed) with 16x25 pixels, each, and two filled silicon bolometer arrays with 16x32 and 32x64 pixels, respectively, to perform integral-field spectroscopy and imaging photometry in the 60-210\mu\ m wavelength regime. In photometry mode, it simultaneously images two bands, 60-85\mu\ m or 85-125\mu\m and 125-210\mu\ m, over a field of view of ~1.75'x3.5', with close to Nyquist beam sampling in each band. In spectroscopy mode, it images a field of 47"x47", resolved into 5x5 pixels, with an instantaneous spectral coverage of ~1500km/s and a spectral resolution of ~175km/s. We summarise the design of the instrument, describe observing modes, calibration, and data analysis methods, and present our current assessment of the in-orbit performance of the instrument based on the Performance Verification tests. PACS is fully operational, and the achieved performance is close to or better than the pre-launch predictions.
  • Pulsed laser deposition was employed to grow thin films of the Heusler compounds Co_2MnSi and Co_2FeSi. Epitaxial growth was realized both directly on MgO (100) and on a Cr or Fe buffer layer. Structural analysis by x-ray and electron diffraction shows for both materials the ordered L2_1 structure. Bulk magnetization was determined with a SQUID magnetometer. The values agree with the Slater-Pauling rule for half-metallic Heusler compounds. On the films grown directly on the substrate measurements of the Hall effect have been performed. The normal Hall effect is nearly temperature independent and points towards a compensated Fermi surface. The anomalous contribution is found to be dominated by skew scattering. A remarkable sign change of both normal and anomalous Hall coefficients is observed on changing the valence electron count from 29 (Mn) to 30 (Fe).
  • Co$_2$FeSi(100) films with L2$_1$ structure deposited onto MgO(100) were studied exploiting both longitudinal (LMOKE) and quadratic (QMOKE) magneto-optical Kerr effect. The films exhibit a huge QMOKE signal with a maximum contribution of up to 30 mdeg, which is the largest QMOKE signal in reflection that has been measured thus far. This large value is a fingerprint of an exceptionally large spin-orbit coupling of second or higher order. The Co$_2$FeSi(100) films exhibit a rather large coercivity of 350 and 70 Oe for film thicknesses of 22 and 98 nm, respectively. Despite the fact that the films are epitaxial, they do not provide an angular dependence of the anisotropy and the remanence in excess of 1% and 2%, respectively.
  • A Co$_2$FeSi (CFS) film with L2$_1$ structure was irradiated with different fluences of 30 keV Ga$^+$ ions. Structural modifications were subsequently studied using the longitudinal (LMOKE) and quadratic (QMOKE) magneto-optical Kerr effect. Both the coercivity and the LMOKE amplitude were found to show a similar behavior upon irradiation: they are nearly constant up to ion fluences of $\approx6\times10^{15}$ ion/cm$^2$, while they decrease with further increasing fluences and finally vanish at a fluence of $\approx9\times10^{16}$ ion/cm$^2$, when the sample becomes paramagnetic. However, contrary to this behavior, the QMOKE signal nearly vanishes even for the smallest applied fluence of $3\times10^{14}$ ion/cm$^2$. We attribute this reduction of the QMOKE signal to an irradiation-induced degeneration of second or higher order spin-orbit coupling, which already happens at small fluences of 30 keV Ga$^+$ ions. On the other hand, the reduction of coercivity and LMOKE signal with high ion fluences is probably caused by a reduction of the exchange interaction within the film material.
  • We report the deposition of thin Co$_2$FeSi films by RF magnetron sputtering. Epitaxial (100)-oriented and L2$_1$ ordered growth is observed for films grown on MgO(100) substrates. (110)-oriented films on Al$_2$O$_3$(110) show several epitaxial domains in the film plane. Investigation of the magnetic properties reveals a saturation magnetization of 5.0 $mu_B/f.u.$ at low temperatures. The temperature dependence of the resistivity $rho_{xx}(T)$ exhibits a crossover from a T^3.5 law at T<50K to a T^1.65 behaviour at elevated temperatures. $rho_{xx}(H)$ shows a small anisotropic magnetoresistive effect. A weak dependence of the normal Hall effect on the external magnetic field indicates the compensation of electron and hole like contributions at the Fermi surface.
  • We have grown thin films of the Heusler compound Co_2FeSi by RF magnetron sputtering. On (100)-oriented MgO substrates we find fully epitaxial (100)-oriented and L2_1 ordered growth. On Al_2O_3 (11-20) substrates, the film growth is (110)-oriented, and several in-plane epitaxial domains are observed. The temperature dependence of the electrical resistivity shows a power law with an exponent of 7/2 at low temperatures. Investigation of the bulk magnetic properties reveals an extrapolated saturation magnetization of 5.0 mu_B/fu at 0 K. The films on Al_2O_3 show an in-plane uniaxial anisotropy, while the epitaxial films are magnetically isotropic in the plane. Measurements of the X-ray magnetic circular dichroism of the films allowed us to determine element specific magnetic moments. Finally we have measured the spin polarization at the surface region by spin-resolved near-threshold photoemission and found it strongly reduced in contrast to the expected bulk value of 100%. Possible reasons for the reduced magnetization are discussed.
  • The Heusler alloy is used as an electrode of magnetic tunneling junctions. The junctions are deposited by magnetron dc sputtering using shadow mask techniques with AlO_{x} as a barrier and cobalt as counter electrode. Measurements of the magnetoresistive differential conductivity in a temperature range between 4K and 300K are shown. An analysis of the barrier properties applying the Simmons model to the bias dependent junction conductivity is performed. VSM measurements were carried out to examine the magnetic properties of the samples.
  • We present a new experiment on YBa_2Cu_3O_{7-x} (YBCO) thin films using spatially resolved heavy ion irradiation. Structures consisting of a periodic array of strong and weak pinning channels were created with the help of metal masks. The channels formed an angle of +/-45 Deg with respect to the symmetry axis of the photolithographically patterned structures. Investigations of the anisotropic transport properties of these structures were performed. We found striking resemblance to guided vortex motion as it was observed in YBCO single crystals containing an array of unidirected twin boundaries. The use of two additional test bridges allowed to determine in parallel the resistivities of the irradiated and unirradiated parts as well as the respective current-voltage characteristics. These measurements provided the input parameters for a numerical simulation of the potential distribution of the Hall patterning. In contrast to the unidirected twin boundaries in our experiment both strong and weak pinning regions are spatially extended. The interfaces between unirradiated and irradiated regions therefore form a Bose-glass contact. The experimentally observed magnetic field dependence of the transverse voltage vanishes faster than expected from the numerical simulation and we interpret this as a hydrodynamical interaction between a Bose-glass phase and a vortex liquid.
  • We suceeded in the preparation of polycrystalline Ca_2FeReO_6 which has a Curie temperature of 540 K, the highest value of all magnetic perovskites investigated up to now. This material has been characterised by X-ray and neutron powder diffraction. We found at 548 K a monoclinic unit cell (space group P2_1/n) with a=5.4366(5) A, b=5.5393(5) A, c=7.7344(5) A, and beta=90.044(4) deg. For low temperatures a phase separation in two monoclinic phases with identical cell volume is observed in neutron scattering. The two phases possess different magnetic structure and coercivity. 57-Fe-Moessbauer spectroscopy measurements show the presence of four different Fe(3+) positions indicating two different phases at room temperature, indistinguishable in the diffraction experiments. The conductivity is thermally activated for all temperatures and no significant magnetoresistivity is observed.
  • We have investigated the crystal structure and the ferroelectric properties of BaTiO3 thin films with YBa2Cu3O7-d as the bottom and Au as the top electrode. Epitaxial heterostructures of YBa2Cu3O7-d and BaTiO3 were prepared by dc and rf sputtering, respectively. The crystal structure of the films was characterised by x-ray diffraction. The ferroelectric behaviour of the BaTiO3 films was confirmed by hysteresis loop measurements using a Sawyer Tower circuit. We obtain a coercive field of 30 kV/cm and a remanent polarisation of 1.25 \muC/cm. At sub-switching fields the capacitance of the films obeys a relation analogous to the Rayleigh law. This behaviour indicates an interaction of domain walls with randomly distributed pinning centres. At a field of 5 MV/m we calculate 3% contribution of irreversible domain wall motion to the total dielectric constant.
  • By pulsed-laser deposition epitaxial thin films of Sr_2FeMoO_6 have been pre- pared on (100) SrTiO_3 substrates. Already for a deposition temperature of 320 C epitaxial growth is achieved. Depending on deposition parameters the films show metallic or semiconducting behavior. At high (low) deposition temperature the Fe,Mo sublattice has a rock-salt (random) structure. The metallic samples have a large negative magnetoresistance which peaks at the Curie temperature. The magnetic moment was determined to 4 mu_B per formula unit (f.u.), in agreement with the expected value for an ideal ferrimagnetic arrangement. We found an ordinary Hall coefficient of -6.01x10^{-10} m^3/As at 300 K, corresponding to an electronlike charge-carrier density of 1.3 per Fe,Mo-pair. In the semiconducting films the magnetic moment is reduced to 1 mu_B/f.u. due to disorder in the Fe,Mo sublattice. In low fields an anomalous holelike contribution dominates the Hall voltage, which vanishes at low temperatures for the metallic films only.
  • We prepared high epitaxial thin films of the compound Sr_2FeMoO_6 with narrow rocking curves by pulsed laser deposition. The diagonal and nondiagonal elements of the resistivity tensor were investigated at temperatures from 4 K up to room temperature in magnetic fields up to 8 T. An electronlike ordinary Hall effect and a holelike anomalous Hall contribution are observed. Both coefficients have reversed sign compared to the colossal magnetoresistive manganites. We found at 300 K an ordinary Hall coefficent of -1.87x10^{-10} m^3/As, corresponding to a nominal charge carrier density of four electrons per formula unit. At low temperature only a small negative magnetoresistance is observed which vanishes at higher temperatures. The temperature coefficient of the resistivity is negative over the whole temperature range. A Kondo like behavior is observed below 30 K while above 100 K variable range hopping like transport occurs.
  • The absolute values of the conductivity in the normal state sigma_n and of the low temperature penetration depths lambda(0) were measured for a number of different samples of the YBaCuO family. We found a striking correlation between sigma_n and 1/lambda^2, regardless of doping, oxygen reduction or defects, thus providing a simple method to predict the superconducting penetration depth and to have an estimate of the sample quality by measuring the normal-state conductivity.
  • We measured the temperature dependence of the linear high field Hall resistivity of La_0.67Ca_0.33MnO_3 (T_C=232K) and La_0.67Sr_0.33MnO_3 (T_C=345K) thin films in the temperature range from 4K up to 360K in magnetic fields up to 20T. At low temperatures we find a charge carrier density of 1.3 and 1.4 holes per unit cell for the Ca- and Sr-doped compound, respectively. In this temperature range electron-magnon scattering contributes to the longitudinal resistivity. At the ferromagnetic transition temperature T_C a dramatic drop in the number of current carriers $n$ down to 0.6 holes per unit cell, accompanied by an increase in unit cell volume, is observed. Corrections of the Hall data due to a non saturated magnetic state will lead a more pronounced charge carrier density collapse.
  • By laser ablation we prepared thin films of the colossal magnetoresistive compound La_(1-x)Ca_xMnO_3 with doping levels 0.1<x<0.9 on MgO substrates. X-ray diffraction revealed epitaxial growth and a systematic decrease of the lattice constants with doping. The variation of the transport and magnetic properties in this doping series was investigated by SQUID magnetization and electrical transport measurements. For the nonmetallic samples resistances up to 10^13 Ohm have been measured with an electrometer setup. While the transport data indicate polaronic transport for the metallic samples above the Curie temperature the low doped ferromagnetic insulating samples show a variable range hopping like transport at low temperature.